    Seawater reverse osmosis systems place extremely high demands on the metallurgical properties of piping materials. High-pressure pumps force corrosive seawater through semipermeable membranes at pressures as high as 85 bar. Standard stainless steel simply cannot withstand such intense chloride exposure and mechanical stress. Even a pinhole leak can disrupt freshwater production and damage expensive plant equipment. As a specialized manufacturer of stainless steel piping, we provide comprehensive guidance on pressure zoning, PREN calculations, alloy grades, and testing procedures.
    SWRO Desalination

    Tabla de contenido

    Why Plant Zones Dictate Pipes for SWRO Desalination

    A single material specification cannot be used throughout the entire plant because modern desalination facilities operate across four distinct hydraulic and chemical zones.
    Raw ocean water enters the plant at low pressure below 6 bar. Total Dissolved Solids (TDS) sit between 35,000 ppm and 45,000 ppm.
    Positive displacement or centrifugal pumps boost feedwater pressure to 60 or 85 bar. Piping in this zone requires massive mechanical tensile strength and pitting immunity.
    Reverse osmosis membranes reject concentrated salt brine at pressures exceeding 60 bar. Salinity spikes to 70,000 or 80,000 ppm TDS inside Energy Recovery Device (ERD) headers. This hyper-saline stream represents the most corrosive environment inside the entire facility.
    Desalinated water leaves the membranes with less than 500 ppm TDS at low pressure.

    SWRO Operating Zones and Piping Requirements

    SWRO Plant ZoneOperating PressureSalinity (TDS)Primary Material Choice
    Seawater Intake1 to 6 bar35,000 to 45,000 ppmHDPE or GRP
    High-Pressure RO Feed60 to 85 bar35,000 to 45,000 ppmSúper Dúplex 2507
    Brine Reject / ERD55 to 80 bar65,000 to 80,000 ppmSuper Duplex 2507 / 6Mo
    Permeate Output1 to 4 barUnder 500 ppm316L Stainless or PVC
    Qué hacemos
    • Plato
    • Hoja
    • Piezas forjadas
    • Barra redonda
    • Brida
    • Tuberías
    • Accesorios
    • Personalizado

    Más información 

    Calculating PREN for Pipes for SWRO Desalination

    Chloride ions attack passive metal films through localized pitting and tight flange crevices. Metallurgists measure chloride resistance using the Índice de resistencia a la corrosión por picaduras (PREN).
    To ensure safe and continuous operation, the PREN value of pipes used to transport raw seawater must be at least 40. However, standard Tubos de acero inoxidable 316L have a PREN value of only 24 and are prone to severe corrosión en grietas after just a few weeks of contact with raw seawater. Even duplex 2205 pipe, with a PREN value of 35, struggles to withstand corrosion in the warm Middle Eastern seawater at temperatures above 30°C. When selecting metal piping for SWRO systems, a PREN value greater than 42 is typically required.So, which pipes have a PREN value higher than 42 and are suitable for SWRO?Let’s take a look.

    Top Metallic Alloys for High-Pressure RO Trains

    Currently, the specifications of seawater desalination equipment worldwide are primarily based on the following three specialized stainless steel series.

    Súper Dúplex 2507

    Tubo Super Duplex 2507 serves as the global benchmark for high-pressure pipes for SWRO desalination.Its PREN value exceeds 42, and its yield strength reaches 550 MPa. The strength of 2507 is twice that of austenitic stainless steel, allowing it to be fabricated into pipes with thinner walls, reducing the overall weight of the pipes by 35% and significantly lowering welding labor costs.

    Super Duplex Zeron 100

    Zeron 100 pipe incorporates 0.5% to 1.0% copper and tungsten into a standard super duplex stainless steel matrix, which enhances resistance to crevice corrosion in static, warm brine pipelines. Stainless steel conforming to the ASTM A790 UNS S32760 standard is ideally suited for service in the Arabian Gulf region, where water temperatures exceed 35°C.

    6Mo Super Austenitic

    Also known as 254 SMO steel pipe, it has a PREN value of 43. It offers excellent formability and weldability, making it suitable for the manufacture of complex instrumentation piping and pump manifolds. However, its yield strength of 300 MPa requires thicker walls than 2507 super duplex steel when operating at a pressure of 80 bar.
    Grado de aleaciónNúmero UNSMinimum PRENFuerza de producciónASTM Pipe Standard
    316LS3160324170 MPaASTM A312
    Dúplex 2205S3220535450 MPaASTM A790
    254 SMOS3125443300 MPaASTM A312
    Súper Dúplex 2507S3275042.5550 MPaASTM A790
    Zeron 100S3276042.5550 MPaASTM A790

    As a professional and reliable manufacturer of stainless steel pipes in China,Kaysuns can not only help you avoid most mistakes when purchasing stainless steel pipes,but we also offer one-stop piping system services to eliminate all purchasing hurdles for you.Feel free to contact us at any time for a free and quick quote.

    Más información 

    Non-Metallic vs Metallic Pipes for SWRO Desalination

    SWRO desalination requires a strategic combination of non-metallic and metallic piping. High-density polyethylene (HDPE) or glass-reinforced plastic (GRP) pipes can be installed in low-pressure feedwater zones. Plastic pipes used in SWRO desalination never rust and cost far less than superalloys.
    Plastic cannot safely withstand pressures of 80 bar without thick walls and bulky supports, and high-pressure GRP fittings are also prone to mechanical fatigue during the daily start-up cycles of the pumps. It is recommended that plants use non-metallic piping for pressures below 10 bar, Super Duplex 2507 for pressures above 16 bar, and 316L stainless steel for low-pressure permeate piping after desalination.

    Welding and Quality Testing for SWRO Piping

    Improper on-site welding can immediately compromise the corrosion resistance of expensive super duplex steel pipes. Excessively high welding temperatures can disrupt the 50/50 austenite-ferrite phase balance and cause the precipitation of brittle σ phase. Order pre-welded products from Kaysuns today! Kaysuns strictly adheres to welding and inspection standards when manufacturing piping for seawater desalination systems.
    • Superalloy Filler Wire:
      Welders use ER2594 TIG filler wire, which contains additional nickel, to stabilize austenite formation in the molten pool.
    • Nitrogen-Mixed Purge:
      Adding 2% nitrogen to pure argon shielding gas prevents nitrogen loss from the root of the weld.
    • Interpass Temperature Control:
      Technicians use digital high-temperature meters to monitor the weld joint, strictly maintaining the interpass temperature below 150°C.
    • Decapado y pasivación:
      A nitric acid–hydrofluoric acid bath removes heat-colored discoloration and fully restores the protective chromium oxide film.
    As a reputable manufacturer of stainless steel pipes in China, we conduct ASTM G48 Method A testing on all SWRO pipes. Laboratory technicians immerse pipe samples in a ferric chloride solution at 50°C for 24 hours. To pass certification, the samples must show no pitting corrosion and exhibit negligible weight loss.

    Mandatory Quality Control Tests for SWRO Pipes

    Inspection TestCódigo estándarTarget Material FlawAcceptance Requirement
    Ferric Chloride PittingASTM G48 Method AIntermetallic phase pittingZero pits at 50°C for 24h
    Ferrite Content CheckASTM E562Austenite-ferrite imbalance35% to 55% Ferrite phase
    Resistencia al impactoASTM A370Brittle fracture riskMin 45 Joules at -46°C
    Radiografía (RT)ASME Sec VIIIInternal weld seam porosity100% X-ray pass on welds

    FAQs on Pipes for SWRO Desalination

    Raw seawater contains 19,000 ppm of aggressive chlorides, while 316L only has a PREN of 24. Chlorides break down the passive layer inside flange crevices, causing rapid pinhole leaks within months. Only use 316L for post-membrane permeate water lines with low salinity.
    Duplex 2205 works only in cold-water brackish plants or low-salinity pre-treatment lines below 20°C. For standard seawater reverse osmosis trains and brine lines, you must specify Super Duplex 2507 (PREN over 42) to prevent crevice corrosion.
    High-pressure roll-grooved couplings allow fast field assembly and reduce costly on-site TIG welding hours. They also isolate pump vibrations and allow easy membrane housing maintenance. Always specify Super Duplex couplings with EPDM gaskets to match the pipe metallurgy.
    As a reliable stainless steel manufacturer, we provide you with a MTC compliant with EN 10204, Section 3.1 or 3.2, which includes the furnace number. We ensure that the certificate contains PMI chemical composition analysis results, an ASTM G48 pitting corrosion test report, ferrite content measurement results, and records of 100% radiographic testing of welds.

    Contacto

    Póngase en contacto con nosotros
    Encuéntranos
    logotipo de Kaysuns

    Póngase en contacto con nosotros

    Suministro de
    Tuberías de acero inoxidable y aleaciones

    • ¿Necesita una oferta?
    • ¿Desea conocer la dimensión / catálogo?
    • ¿Hablamos de cuestiones técnicas?

    No dude en ponerse en contacto con nosotros, estaremos encantados de responder a todas sus preguntas.

    Obtenga ahora un presupuesto gratuito

    small_c_popup.png

    Solicite ahora un presupuesto gratuito