Common Materials for an ASTM A269 Tube
Manufacturing Processes and Sizing Specifications
Standard Outside Diameter Tolerances for ASTM A269 Tube
| Specified OD | OD Tolerance (Imperial) | OD Tolerance (Metric Equivalent) | Nominal Wall Thickness Tolerance |
|---|---|---|---|
| Under 1/2” 12.7 mm | ± 0.005 in. | ± 0.13 mm | ± 15% |
| 1/2” to 1-1/2” 12.7 to 38.1 mm | ± 0.005 in. | ± 0.13 mm | ± 10% |
| Over 1-1/2” to 3-1/2” 38.1 to 88.9 mm | ± 0.010 in. | ± 0.25 mm | ± 10% |
| Over 3-1/2” to 5-1/2” 88.9 to 139.7 mm | ± 0.015 in. | ± 0.38 mm | ± 10% |
| Over 5-1/2” to 8” 139.7 to 203.2 mm | ± 0.030 in. | ± 0.76 mm | ± 10% |
Ovality of ASTM A269 Tube
- Standard Wall Thickness (>3% of OD):
For standard tubing,the maximum and minimum diameter measurements at any given cross-section must fall entirely within the standard outside diameter tolerance range specified above.No additional ovality tolerance is provided. - Thin-walled tubes (≤ 3% of OD):
Tubes with wall thicknesses less than or equal to 3% of the outside diameter are subject to natural deformation during heat treatment.For such thin-walled tubes,the permissible ovality range is expanded to twice the standard outside diameter tolerance range.However,the average of the maximum and minimum outside diameter readings must still comply with the primary tolerance.
O que fazemos
- Placa
- Folha
- Forjados
- Barra redonda
- Mesa
- Tubos
- Conexões
- Personalizado
Entre em contato conosco para obter mais informações
Key Mechanical Properties of the ASTM A269 Tube
Maximum Hardness Limits for Common Grades
| Grau de aço inoxidável | Brinell HBW, Max | Rockwell, Max | Vickers HV, Max |
|---|---|---|---|
| TP304 / TP304L | 192 HBW | 90 HRB | 200 HV |
| TP316 / TP316L | 192 HBW | 90 HRB | 200 HV |
| TP321 (Stabilized) | 192 HBW | 90 HRB | 200 HV |
| TP347 | 192 HBW | 90 HRB | 200 HV |
| TP317L | 192 HBW | 90 HRB | 200 HV |
| TP201 | 220 HBW | 96 HRB | 230 HV |
| TP201LN | 250 HBW | 100 HRB | 263 HV |
| TPXM-10 | 269 HBW | 25 HRC | 285 HV |
Primary Application Fields Worldwide
Required Testing and Quality Control Standards
ASTM A269 Tube Specification:Quality Control Test Methods
| Test Category | Specific Test Method | Reference Standard Parâmetro | Purpose & Acceptance Criteria |
|---|---|---|---|
| Mechanical Destructive | Teste de dureza | ASTM E18 Max 90 HRB 192 HBW | Ensures the tube is fully solution-annealed and ductile. Exempt for tubes < 1/4" ID or < 0.020" wall. |
| Teste de Flaring (Seamless) | ASTM A1016 Tapered mandrel | Expands the tube end. The material must show no visible cracking or structural tearing. | |
| Teste de Flange (Soldado) | ASTM A1016 90° bend flange | Forms a flat rim at the tube edge. Checks for seam split or heat-affected zone (HAZ) cracking. | |
| Achatamento reverso (Soldado) | ASTM A1016 180° split & flatten | Evaluates internal weld root penetration. The flattened weld section must show no signs of separation. | |
| Nondestructive | Teste de corrente parasita | ASTM E426 Electromagnetic coils | Detects subsurface micro-defects,pinholes, or cracks by scanning changes in electrical conductivity. |
| Teste Hidrostático | ASTM A1016 Calculated pressure | Presses water into the tube to verify mechanical leak tightness. Must hold pressure without drops or sweat. | |
| Dimensional Checks | Diâmetro Exterior | Caliper Laser micrometer | Verifies strict exterior dimensions(e.g., ±0.005″ for 1/2″ to 1-1/2″ tubes) for proper fitting connection. |
| Espessura da parede | Ball micrometer Ultrassônico | Ensures consistency across the lot (typically ±10% for standard sizes, ±15% for < 1/2" OD). | |
| Metalúrgico Químico | Análise química | OES Espectrometria | Verifies that alloy elements (C, Cr, Ni, Mo, etc.) precisely match the mandatory UNS chemistry limits. |
| Grain Size Exam | ASTM E112 Microestrutura | Evaluates crystalline grain refinement under magnification to confirm proper heat treatment. |
Proper Installation of an ASTM A269 Tube
ASTM A269 Tube Troubleshooting
Não,você nunca deve utilizá-lo em estruturas que suportam carga. Esta especificação destina-se exclusivamente a aplicações de transporte de fluidos e de uso geral. Para fins estruturais mecânicos, você deve optar pelos tubos ASTM A554.
A norma ASTM A213 se aplica especificamente a tubos para caldeiras e trocadores de calor que operam em altas temperaturas. Ela exige a realização contínua de ensaios rigorosos de tração. Por outro lado, a norma ASTM A269 destina-se a ambientes de serviço geral e exige apenas ensaios de dureza.
A norma exige apenas que os tubos estejam limpos e livres de incrustações. É possível solicitar separadamente polimentos especiais de espelho para aplicações de contato com alimentos.
Sim,austenitic stainless steel retains excellent toughness at ultra-low temperatures.Aerospace and medical industries use them safely for liquid nitrogen transport lines.
Contate-nos
- RM901 No.22 Tangjiaqiao Road Wenzhou China
- +86 577 8551 1171
- [email protected]
- https://www.kaysuns.com/