Inconel 600 Plate
Core Properties of Inconel 600 Plate
- Thermal Capabilities:
The alloy has a melting range of 1354°C to 1413°C (2470°F to 2575°F).It maintains mechanical integrity,strength,and oxidation resistance up to 1093°C (2000°F). - Résistance à la corrosion :
It performs well in both oxidizing conditions and reducing environments.It holds up exceptionally well against organic acids,alkaline solutions,and nitriding/carburizing atmospheres. - Résistance mécanique :
In its hot-rolled annealed condition,it typically features a minimum yield strength of 30–45 ksi (205–310 MPa) and a tensile strength of 80–100 ksi (550–725 MPa). - Magnetism:
It is virtually non-magnetic at room temperature.

Applications of Inconel 600 Plate
- Jet engines
- Rocket motors
- Systèmes d'échappement
- Combustion liners
- Reactor vessels
- Distillation columns
- Heating elements
- Industrial baskets
- Reactor cores
- Steam generators
- Control rods
- Waste containers
Chemical Composition of Inconel 600 Plate
| Ni + Co | Cr | Fe | Mn | C | Si | Cu | S |
|---|---|---|---|---|---|---|---|
| ≥ 72.0 | 14,0 – 17,0 | 6,0 – 10,0 | ≤ 1.0 | ≤ 0.15 | ≤ 0.50 | ≤ 0.50 | ≤ 0,015 |
Rôle des éléments clés
- Nickel:
Functions as the base matrix element.It gives the plate superb resistance to reducing environments,keeps it ductile at cryogenic temperatures,and makes it virtually immune to chloride-ion stress corrosion cracking. - Chrome:
Provides high-temperature oxidation protection by forming a stable,microscopic protective film on the plate surface.It also protects the material from sulfur and acidic compounds. - Le fer:
Balances out the crystalline structure.It assists the nickel core in providing excellent mechanical strength and helps lower total manufacturing costs.
Inconel 600 Standards & Equivalent Designations
| Inconel 600 Alloy | |||||
|---|---|---|---|---|---|
| Standard / System | Equivalent Designation | Forme du produit | ASTM | ASME | SAE AMS |
| Numéro UNS | UNS N06600 | Plates, Sheets & Strips | ASTM B168 | ASME SB168 | AMS 5540 |
| DIN / German Werkstoff | W.Nr. 2.4816 | Bars, Rods, Wires & Shapes | ASTM B166 | ASME SB166 | AMS 5665 / AMS 5687 |
| EN Chemical Name | NiCr15Fe | Seamless Pipes & Tubes | ASTM B167 | ASME SB167 | – |
| JIS | NCF 600 | Condenser & Heat Exchanger Tubes | ASTM B163 | ASME SB163 | – |
| BS | NA 14 | Welded Pipes & Tubes | ASTM B516 / B517 | ASME SB516 / SB517 | – |
| AFNOR | NC15Fe | Forgings & Flanges / Fittings | ASTM B564 | ASME SB564 | AMS 5665 |
| Generic Trade Name | Alloy 600, Inconel 600 | ||||
Vous avez un besoin ?
Contactez-nous pour plus d'informations
Mechanical Properties of Inconel 600 Plate
Room-Temperature Mechanical Properties
| Biens | Hot-Rolled Annealed Plate | Cold-Rolled Annealed Plate |
|---|---|---|
| Résistance à la traction | ≥ 550 MPa (80 ksi) | ≥ 550 MPa (80 ksi) |
| Limite d'élasticité | ≥ 205 MPa (30 ksi) | ≥ 240 MPa (35 ksi) |
| Élongation | ≥ 35% | ≥ 30% |
| Dureté | ≤ 85 HRB | ≤ 92 HRB |
Performance mécanique à haute température
Inconel 600 is selected for engineering designs because it retains structural strength and resists “creep” (gradual deformation under constant load) at elevated temperatures.
- At 540°C (1000°F):
Yield strength drops only slightly to approximately 24 ksi (165 MPa),and tensile strength remains robust around 75 ksi (517 MPa). - At 760°C (1400°F):
The material still holds a tensile strength of roughly 25 ksi (172 MPa),allowing it to function under structural loads where standard stainless steels soften or scale.
Cryogenic Performance & Impact Toughness
Inconel 600 does not exhibit a ductile-to-brittle transition point at low temperatures.
- Cryogenic Strength:
At sub-zero temperatures (down to -196°C / -320°F),its tensile and yield strengths actually increase significantly,while its ductility drops only marginally. - Impact Toughness:
Charpy V-Notch testing results for annealed plates typically exceed 150 ft-lbs (203 J) at room temperature and remain virtually unchanged at cryogenic temperatures,making it highly resistant to catastrophic fracturing.
Modulus of Elasticity and Fatigue
- Modulus of Elasticity (Tension):
31.0 x 10⁶ psi (214 GPa) at room temperature,providing high structural rigidity. - Fatigue Strength:
The endurance limit for annealed material under reversed bending cycles is roughly 39 ksi (270 MPa) at 10⁸ cycles.
Our Advantages in Manufacturing Inconel 600 Plate
Grain-Size Control via Precision Annealing
Strict mastery over the solid-solution structure through state-of-the-art,atmosphere-controlled annealing furnaces.
Inconel 600 cannot be hardened by heat treatment,meaning its mechanical property balance depends entirely on grain boundary engineering.Your precise thermal profiling prevents grain coarsening.This ensures the plates achieve an optimal balance of high-temperature creep strength and excellent cold formability for your customers.
Surface Cleanliness and Passivation
Implementation of automated descaling and advanced chemical pickling lines tailored specifically for high-nickel chemistries.
To achieve Inconel 600’s signature high-temperature oxidation resistance,the chromium must form an uncompromised,uniform protective oxide film.Your process removes all surface iron contamination and mill scale.This guarantees flawless performance in severe nitriding,carburizing,or corrosive chemical environments.
Gauge Uniformity and Flatness Tollerances
Utilizing high-precision rolling mills equipped with real-time, continuous Automatic Gauge Control (AGC) systems.
Plates destined for aerospace combustion liners,nuclear steam generators,or heavy pressure vessels require strict dimensional accuracy.Your ability to deliver tight thickness tolerances and superior flatness minimizes material waste during CNC cutting and ensures seamless fit-up during robotic or manual welding.
100% Traceability and Nuclear-Grade Quality
Comprehensive,in-house testing protocols fully compliant with ASTM B168,ASME SB168,and Section III/VIII pressure vessel codes.
Every plate is backed by a verifiable material test report detailing chemical analysis,non-destructive testing,and mechanical validation.This provides tier-1 aerospace,chemical processing,and nuclear clients with absolute risk mitigation.
FAQs About Inconel 600 Plate
It can be welded using standard industrial methods like TIG (GTAW),MIG (GMAW),or SMAW.The most critical factor is using matching nickel-alloy consumables to maintain corrosion resistance:
- TIG/MIG Wire:AWS A5.14 ERNiCr-3 (Inconel 82)
- Covered Electrodes:AWS A5.11 ENiCrFe-3 (Inconel 182)