Hastelloy X Pipe Supplier
Приложения

Hastelloy X Equivalent Designations
- UNS N06002
- Сплав X
- DIN 2.4665
- DIN Specification NiCr22Fe18Mo
- AFNOR NC22FeD
- GB GH3536 or GH536
У вас есть требования?
Свяжитесь с нами для получения дополнительной информации
Chemical Composition of Hastelloy X Pipe, wt.%
| Ni | Cr | Fe | Пн | Co | W | Mn | Si | C | п | S | B |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Остаток средств | 20.50 – 23.00 | 17.00 – 20.00 | 8.00 – 10.00 | 0.50 – 2.50 | 0.20 – 1.00 | 1.00 Макс | 1.00 Макс | 0.05 – 0.15 | 0,04 макс. | 0,03 макс. | 0.008 Max |
What is The Purpose of The High Iron (Fe) Content?
How Does Chromium (Cr) Contribute to Its Performance?
Mechanical Properties of Hastelloy X Pipe
| Предел прочности | Предел текучести (смещение 0,2%) | Удлинение | Твердость (макс.) |
|---|---|---|---|
| ≥ 655 MPa(95 ksi) | ≥ 240 MPa(35 ksi) | ≥ 35% | 90 – 95 HRB(180 – 220 HBW) |
High-Temperature Tensile Strength
One of Hastelloy X’s defining features is its ability to retain significant mechanical integrity as temperatures rise.Below is a representation of how its tensile strength behaves at extreme temperatures:
Creep and Stress-Rupture Strength
- In long-term service (e.g., in furnaces and kilns),creep resistance (slow deformation under load) is more critical than instantaneous tensile strength.
- Typical 10,000-hour fracture strength:
At 1500°F (815°C), Hastelloy X alloy can withstand a stress of approximately 8.5 ksi (59 MPa) for up to 10,000 hours before failure. - Ductility Retention:
Unlike many superalloys that become brittle over time,Alloy X exhibits good ductility even after 16,000 hours of exposure to temperatures between 1200℉ and 1600℉.
Hastelloy X Pipe Physical & Thermal Properties
Физические свойства
| Имущество | Metric Value | Imperial Value |
|---|---|---|
| Плотность | 8.22 g/cm3 | 0.297 lb/in3 |
| Диапазон плавления | 1260 – 1355℃ | 2300 – 2470℉ |
| Electrical Resistivity(22℃) | 1.18μΩ · m | 2300 – 2470℉ |
| Magnetic Permeability | < 1.002 | Немагнитный |
| Poisson’s Ratio(22℃) | 0.320 | |
Тепловые свойства
Теплопроводность
- 20°C (70°F): 9.1 W/m·K
- 600°C (1100°F): 20.6 W/m·K
- 900°C (1700°F): 27.4 W/m·K
Коэффициент теплового расширения
- 26–100°C: 13.8 μm/m·K
- 26–500°C: 14.9 μm/m·K
- 26–1000°C: 16.6 μm/m·K
FAQs About Hastelloy X Pipe
Да.It exhibits exceptional resistance to carburization and nitriding,which are the primary causes of failure in other high-temperature alloys used in industrial furnaces and petrochemical plants.
Due to work hardening,it is more difficult to machine than ordinary stainless steel.To machine it successfully,it is necessary to use rigid fixtures,sharp carbide or ceramic cutting tools,and low cutting speeds,while maintaining a constant feed rate to prevent “welding” of the tool to the surface.
Выберите труба из инконеля 625 for applications requiring higher tensile and fatigue strength at moderately high temperatures(1800℉).
Выберите hastelloy X pipe when the environment involves extremely high temperatures (1800 – 2200℉) or specifically requires resistance to carburization.
Связаться с нами
- RM901 No.22 Tangjiaqiao Road Wenzhou Китай
- +86 577 8551 1171
- [email protected]