{"id":48846,"date":"2025-02-20T08:08:58","date_gmt":"2025-02-20T08:08:58","guid":{"rendered":"https:\/\/www.kaysuns.com\/?p=48846"},"modified":"2025-09-19T05:33:15","modified_gmt":"2025-09-19T05:33:15","slug":"uns-n04400-precauciones-e-instrucciones","status":"publish","type":"post","link":"https:\/\/www.kaysuns.com\/es\/uns-n04400-precauciones-e-instrucciones\/","title":{"rendered":"Precauciones de soldadura e instrucciones de proceso para tubos soldados de aleaci\u00f3n UNS N04400"},"content":{"rendered":"<div data-elementor-type=\"wp-post\" data-elementor-id=\"48846\" class=\"elementor elementor-48846\" data-elementor-post-type=\"post\">\n\t\t\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-f9b817a elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"f9b817a\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-3367520\" data-id=\"3367520\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-3ac2d86 elementor-widget elementor-widget-text-editor\" data-id=\"3ac2d86\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p><strong>UNS N04400<\/strong>tambi\u00e9n llamado monel 400,MCu-28-1.5-1.8 o Ni68Cu28Fe. <br \/>Se trata de un <a href=\"\/es\/guia-rapida-de-aleaciones-de-niquel\/\" target=\"_blank\">aleaci\u00f3n a base de n\u00edquel<\/a> material con buena <a href=\"\/es\/aleacion-monel-400-resistente-al-agua-de-mar-y-al-acido-fluorhidrico\/#corrosionResistance\" target=\"_blank\">resistencia a la corrosi\u00f3n<\/a> en agua de mar, disolventes qu\u00edmicos y diversos medios \u00e1cidos.<br \/>Especialmente en resistencia a la corrosi\u00f3n por \u00e1cido fluorh\u00eddrico, ocupa el primer lugar en el ranking general de aleaciones con base de n\u00edquel.<br \/>El principal <a href=\"\/es\/aleacion-monel-400-resistente-al-agua-de-mar-y-al-acido-fluorhidrico\/#chemicalComposition\" target=\"_blank\">componentes<\/a> de Monel 400 son <strong>N\u00cdQUEL<\/strong> y <strong>COBRE<\/strong>.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-f8fb5cf elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"f8fb5cf\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-4608ce3\" data-id=\"4608ce3\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-66eaad2 elementor-widget elementor-widget-heading\" data-id=\"66eaad2\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Precauciones de soldadura para N04400<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-7059fef elementor-widget elementor-widget-text-editor\" data-id=\"7059fef\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Monel 400 tiene un buen rendimiento de soldadura, puede ser TIG y MIG m\u00e9todo, puede utilizar Monel cuerpo o EniCu-7 alambre, electrodo. O manual de soldadura por arco el\u00e9ctrico y soldadura por arco sumergido, se puede soldar con acero al carbono y acero de baja aleaci\u00f3n. Le recordamos los dos puntos siguientes.<\/p><p>Es f\u00e1cil que se produzcan grietas t\u00e9rmicas, especialmente en la fosa de arco, donde la sensibilidad a las grietas es mayor. Principalmente en el pozo de arco S, P segregaci\u00f3n, S, P y Ni forman un co-cristal de bajo punto de fusi\u00f3n. En el proceso de cristalizaci\u00f3n de la soldadura, la segregaci\u00f3n en el l\u00edmite cristalino, bajo la acci\u00f3n de la tensi\u00f3n de tracci\u00f3n para producir grietas. Por lo tanto, el contenido de S, P debe controlarse estrictamente.<\/p><p>El metal l\u00edquido tiene poca fluidez y puede disolver gases como el ox\u00edgeno, el nitr\u00f3geno y el hidr\u00f3geno, por lo que es propenso a la porosidad.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-834c831 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"834c831\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-72c808f\" data-id=\"72c808f\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-3facf9c elementor-cta--skin-classic elementor-animated-content elementor-bg-transform elementor-bg-transform-zoom-in elementor-widget elementor-widget-call-to-action\" data-id=\"3facf9c\" data-element_type=\"widget\" data-widget_type=\"call-to-action.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<a class=\"elementor-cta\" href=\"#elementor-action%3Aaction%3Dpopup%3Aopen%26settings%3DeyJpZCI6IjQ2ODEzIiwidG9nZ2xlIjpmYWxzZX0%3D\">\n\t\t\t\t\t<div class=\"elementor-cta__bg-wrapper\">\n\t\t\t\t<div class=\"elementor-cta__bg elementor-bg\" style=\"background-image: url(https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-CTA.webp);\" role=\"img\" aria-label=\"N04400-CTA\"><\/div>\n\t\t\t\t<div class=\"elementor-cta__bg-overlay\"><\/div>\n\t\t\t<\/div>\n\t\t\t\t\t\t\t<div class=\"elementor-cta__content\">\n\t\t\t\t\n\t\t\t\t\t\t\t\t\t<h2 class=\"elementor-cta__title elementor-cta__content-item elementor-content-item\">\n\t\t\t\t\t\tQu\u00e9 hacemos\t\t\t\t\t<\/h2>\n\t\t\t\t\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-cta__description elementor-cta__content-item elementor-content-item\">\n\t\t\t\t\t\tKAYSUNS proporciona un paquete de soluciones para materiales de tuber\u00edas como tuber\u00edas, accesorios, bridas, v\u00e1lvulas en acero inoxidable, acero d\u00faplex y acero aleado, etc. \t\t\t\t\t<\/div>\n\t\t\t\t\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-cta__button-wrapper elementor-cta__content-item elementor-content-item\">\n\t\t\t\t\t<span class=\"elementor-cta__button elementor-button elementor-size-\">\n\t\t\t\t\t\tContacto\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t\t<\/a>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-1c23362 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"1c23362\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-22b1a88\" data-id=\"22b1a88\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-6723a55 elementor-widget elementor-widget-heading\" data-id=\"6723a55\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">N04400 Soldadura Descripci\u00f3n<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-a8e684f elementor-widget elementor-widget-text-editor\" data-id=\"a8e684f\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Para probar su rendimiento y proceso de soldadura, citamos un ejemplo de cliente para hacer la gu\u00eda de prueba de soldadura.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-7512b89 elementor-widget elementor-widget-heading\" data-id=\"7512b89\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">Especificaciones de la placa de ensayo<\/h3>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-db26437 elementor-widget elementor-widget-text-editor\" data-id=\"db26437\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Dos placas de prueba de 10*300*100, \u00e1ngulo de biselado de soldadura 37,5\u00b0, borde romo 4mm, utilizando un proceso de cepillado. El origen de la placa de prueba es VDM, Alemania.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-f9390e5 elementor-widget elementor-widget-heading\" data-id=\"f9390e5\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">Proceso de soldadura de prueba<\/h3>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-e4074c8 elementor-widget elementor-widget-text-editor\" data-id=\"e4074c8\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>El proceso de soldadura de prueba consiste en biselar primero, ensamblar despu\u00e9s la placa de prueba y soldarla por puntos, a\u00f1adiendo la placa de entrada y salida 304.<br \/>A continuaci\u00f3n, se realiza la limpieza previa a la soldadura para prepararla.<br \/>La soldadura est\u00e1 automatizada, utilizando el proceso PAW para la imprimaci\u00f3n, seguido de tres pasadas de alambre de relleno TIG y soldadura de la cubierta.<br \/>Una vez finalizada la soldadura, se llev\u00f3 a cabo la inspecci\u00f3n RT y se realizaron pruebas mec\u00e1nicas.<br \/>Debido al tama\u00f1o limitado de la placa de prueba, la prueba mec\u00e1nica s\u00f3lo pudo completar la prueba de tracci\u00f3n y la prueba de flexi\u00f3n hacia delante y hacia atr\u00e1s de la soldadura.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-a5ba96d elementor-widget elementor-widget-heading\" data-id=\"a5ba96d\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">Situaci\u00f3n de la soldadura<\/h3>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-2e31879 elementor-widget elementor-widget-text-editor\" data-id=\"2e31879\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>El operario debe operar de forma estandarizada y controlar adecuadamente los par\u00e1metros de soldadura. En este momento, la placa soldada tiene una buena calidad de soldadura y cumple los requisitos de rendimiento de la aleaci\u00f3n N04400.<\/p><p>Utilice <strong>poco calor<\/strong> de entrada para reducir la probabilidad de agrietamiento. <strong>Especificaciones de soldadura bajas<\/strong> (corriente, tensi\u00f3n, velocidad de soldadura) para reducir el riesgo de deformaci\u00f3n y los defectos de soldadura. Control de la temperatura entre capas <strong>menos de 100\u2103<\/strong> para reducir la influencia del ciclo t\u00e9rmico en el proceso de soldadura.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-e117222 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"e117222\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-0eb8d1c\" data-id=\"0eb8d1c\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-0bca85e elementor-widget elementor-widget-image\" data-id=\"0bca85e\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img fetchpriority=\"high\" decoding=\"async\" width=\"1024\" height=\"401\" src=\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471-1024x401.webp\" class=\"attachment-large size-large wp-image-48894\" alt=\"N04400-P1\" srcset=\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471-1024x401.webp 1024w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471-300x117.webp 300w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471-768x301.webp 768w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471-18x7.webp 18w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp 1081w\" sizes=\"(max-width: 1024px) 100vw, 1024px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-1897211 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"1897211\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-3fa617c\" data-id=\"3fa617c\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-8efbc95 elementor-widget elementor-widget-heading\" data-id=\"8efbc95\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">N04400 Proceso de soldadura<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-55bede7 elementor-widget elementor-widget-text-editor\" data-id=\"55bede7\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\u2160, Metal fundido <strong>Composici\u00f3n qu\u00edmica<\/strong> (%)\n<table border=\"1\">\n<thead>\n<tr bgcolor=\"#00a0e9\">\n<th>Designaci\u00f3n<\/th>\n<th>Di\u00e1metro (mm)<\/th>\n<th>C<\/th>\n<th>Minnesota<\/th>\n<th>Si<\/th>\n<th>S<\/th>\n<th>P<\/th>\n<th>Alabama<\/th>\n<th>Fe<\/th>\n<th>Ti<\/th>\n<th>Cu<\/th>\n<th>Ni+Co<\/th>\n<th>Ni<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td bgcolor=\"#05B8E4\">Alambre de soldadura<\/td>\n<td>1.6<\/td>\n<td>0.072<\/td>\n<td>3.53<\/td>\n<td>0.97<\/td>\n<td>0.001<\/td>\n<td>0.005<\/td>\n<td>0.12<\/td>\n<td>0.12<\/td>\n<td>2.35<\/td>\n<td>Resto<\/td>\n<td>65.11<\/td>\n<td>\/<\/td>\n<!-- class=\"diagonal-line\" --><\/tr>\n<tr>\n<td bgcolor=\"#05B8E4\">Varilla de soldadura<\/td>\n<td>3.2<\/td>\n<td>0.10<\/td>\n<td>3.38<\/td>\n<td>0.84<\/td>\n<td>0.003<\/td>\n<td>0.005<\/td>\n<td>0.22<\/td>\n<td>0,45\/td&gt;<\/td>\n<td>0.74<\/td>\n<td>29.52<\/td>\n<td>\/<\/td>\n<!-- class=\"diagonal-line\" -->\n<td>64.74<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\nNota: Alambre de soldadura ERNiCu-7 Monel-60. Varilla de soldadura ENiCu-7 Monel-190.\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-0829347 elementor-widget elementor-widget-text-editor\" data-id=\"0829347\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>\u2161, Varilla de soldadura 350\u2103\u00d71h de secado; alambre prestar atenci\u00f3n a la limpieza de la superficie.Normalmente no precalentamiento en necesario. Precalentar por debajo de 100\u00b0C si es necesario.<\/p><p>\u2162, polaridad de soldadura por arco para conexi\u00f3n inversa DC, TIG para conexi\u00f3n positiva DC, di\u00e1metro de tungsteno conexi\u00f3n positiva, di\u00e1metro de tungsteno \u03c63mm, di\u00e1metro de boquilla \u03c610mm, pureza de arg\u00f3n 99,99%.<\/p><p>\u2163, Afilado mec\u00e1nico y fregar el bisel y su filo con acetona.<\/p><p>V, forma biselada y secuencia de soldadura<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-f052d66 elementor-widget elementor-widget-image\" data-id=\"f052d66\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" width=\"2560\" height=\"584\" src=\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-Bevel-Form-Welding-Sequence.webp\" class=\"attachment-full size-full wp-image-48877\" alt=\"N04400-Forma de nivel y secuencia de soldadura\" srcset=\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-Bevel-Form-Welding-Sequence.webp 2560w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-Bevel-Form-Welding-Sequence-300x68.webp 300w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-Bevel-Form-Welding-Sequence-1024x234.webp 1024w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-Bevel-Form-Welding-Sequence-768x175.webp 768w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-Bevel-Form-Welding-Sequence-1536x350.webp 1536w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-Bevel-Form-Welding-Sequence-2048x467.webp 2048w, https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-Bevel-Form-Welding-Sequence-18x4.webp 18w\" sizes=\"(max-width: 2560px) 100vw, 2560px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-1796f6a elementor-widget elementor-widget-text-editor\" data-id=\"1796f6a\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\u2165, Par\u00e1metros de soldadura\n<table border=\"1\">\n<thead>\n<tr bgcolor=\"#00a0e9\">\n<th>M\u00e9todo de soldadura<\/th>\n<th>Niveles de soldadura<\/th>\n<th>Corriente de soldadura (A)<\/th>\n<th>Tensi\u00f3n del arco (V)<\/th>\n<th>Velocidad de soldadura (cm\/min)<\/th>\n<th>12<\/th>\n<th>Caudal de arg\u00f3n (L\/min)<\/th>\n<th>Temperatura entre capas ( \u00b0C)<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td bgcolor=\"#05B8E4\">TIG<\/td>\n<td>Capa inferior<\/td>\n<td>70 ~ 120<\/td>\n<td>14 ~ 18<\/td>\n<td>10<\/td>\n<td>10080<\/td>\n<td>8 ~ 12<\/td>\n<td>\/<\/td>\n<\/tr>\n<tr>\n<td bgcolor=\"#05B8E4\">TIG<\/td>\n<td>Segundo<\/td>\n<td>95 ~ 120<\/td>\n<td>14 ~ 18<\/td>\n<td>6<\/td>\n<td>15400<\/td>\n<td>8 ~ 12<\/td>\n<td>Menos del 100<\/td>\n<\/tr>\n<tr>\n<td bgcolor=\"#05B8E4\">Soldadura por arco manual<\/td>\n<td>Capa de cubierta<\/td>\n<td>110 ~ 120<\/td>\n<td>22 ~ 24<\/td>\n<td>7<\/td>\n<td>20740<\/td>\n<td>\/<\/td>\n<td>Menos del 100<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-fd8974e elementor-widget elementor-widget-text-editor\" data-id=\"fd8974e\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>VIII, El alambre de relleno debe mantenerse en un \u00e1ngulo adecuado para una alimentaci\u00f3n r\u00e1pida.<\/p><p>\u2168, Controle la profundidad de fusi\u00f3n durante la aplicaci\u00f3n y mantenga la relaci\u00f3n de fusi\u00f3n por debajo de 50%. Utilice tambi\u00e9n una corriente baja.<\/p><p>\u2169, Las trayectorias de soldadura estrechas y planas son las mejores. Las piezas de soldadura frontal elevadas deben minimizar el volumen del ba\u00f1o de fusi\u00f3n, para facilitar la conformaci\u00f3n de la soldadura. Al cerrar el arco, prestar atenci\u00f3n a llenar la fosa del arco.<\/p><p>\u216a, Utilice soldadura de arco corto para evitar la ingesta excesiva de gases nocivos durante el proceso de soldadura.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-fd6a1fc elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"fd6a1fc\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-854686f\" data-id=\"854686f\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-dc3ba38 elementor-widget elementor-widget-text-editor\" data-id=\"dc3ba38\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Puede que tambi\u00e9n quiera leer:<br \/><a href=\"https:\/\/www.kaysuns.com\/es\/el-arte-y-la-ciencia-de-la-soldadura-de-tuberias\/\" target=\"_blank\" rel=\"noopener\">El arte y la ciencia de la soldadura de tuber\u00edas<\/a><\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<\/div>","protected":false},"excerpt":{"rendered":"<p>UNS N04400, tambi\u00e9n llamado monel 400,MCu-28-1.5-1.8 o Ni68Cu28Fe. Es un material de aleaci\u00f3n a base de n\u00edquel con buena resistencia a la corrosi\u00f3n en agua de mar, disolventes qu\u00edmicos y diversos medios \u00e1cidos, especialmente en la resistencia a la corrosi\u00f3n del \u00e1cido fluorh\u00eddrico, ocupando el primer lugar en las aleaciones a base de n\u00edquel en general. Precauciones de soldadura para N04400 Monel 400 tiene buena...&nbsp;<a href=\"https:\/\/www.kaysuns.com\/es\/uns-n04400-precauciones-e-instrucciones\/\" rel=\"bookmark\">Leer m\u00e1s \"<span class=\"screen-reader-text\">Precauciones de soldadura e instrucciones de proceso para tubos soldados de aleaci\u00f3n UNS N04400<\/span><\/a><\/p>","protected":false},"author":1,"featured_media":48894,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"neve_meta_sidebar":"","neve_meta_container":"","neve_meta_enable_content_width":"","neve_meta_content_width":0,"neve_meta_title_alignment":"","neve_meta_author_avatar":"","neve_post_elements_order":"","neve_meta_disable_header":"","neve_meta_disable_footer":"","neve_meta_disable_title":"","neve_meta_reading_time":"","_ti_tpc_template_sync":false,"_ti_tpc_template_id":"","footnotes":""},"categories":[316,186],"tags":[],"class_list":["post-48846","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-blog","category-stainless-steel-knowledge"],"yoast_head":"<!-- This site is optimized with the Yoast SEO plugin v26.6 - https:\/\/yoast.com\/wordpress\/plugins\/seo\/ -->\n<title>N04400 Welding Precautions And Process Instructions<\/title>\n<meta name=\"description\" content=\"UNS N04400 is a nickel-based alloy material with good welding performance. We introduce you to its welding precautions.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/www.kaysuns.com\/es\/uns-n04400-precauciones-e-instrucciones\/\" \/>\n<meta property=\"og:locale\" content=\"es_ES\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"N04400 Welding Precautions And Process Instructions\" \/>\n<meta property=\"og:description\" content=\"UNS N04400 is a nickel-based alloy material with good welding performance. We introduce you to its welding precautions.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/www.kaysuns.com\/es\/uns-n04400-precauciones-e-instrucciones\/\" \/>\n<meta property=\"og:site_name\" content=\"Stainless Steel Pipe and Fittings | KAYSUNS\" \/>\n<meta property=\"article:published_time\" content=\"2025-02-20T08:08:58+00:00\" \/>\n<meta property=\"article:modified_time\" content=\"2025-09-19T05:33:15+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp\" \/>\n\t<meta property=\"og:image:width\" content=\"1081\" \/>\n\t<meta property=\"og:image:height\" content=\"423\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/webp\" \/>\n<meta name=\"author\" content=\"admin\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:creator\" content=\"@Admin\" \/>\n<meta name=\"twitter:label1\" content=\"Escrito por\" \/>\n\t<meta name=\"twitter:data1\" content=\"admin\" \/>\n\t<meta name=\"twitter:label2\" content=\"Tiempo de lectura\" \/>\n\t<meta name=\"twitter:data2\" content=\"4 minutos\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\/\/schema.org\",\"@graph\":[{\"@type\":\"Article\",\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#article\",\"isPartOf\":{\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/\"},\"author\":{\"name\":\"admin\",\"@id\":\"https:\/\/www.kaysuns.com\/#\/schema\/person\/9dd889bbe4a74acafea3a8d6480ae741\"},\"headline\":\"UNS N04400 Alloy Welded Pipe Welding Precautions And Process Instructions\",\"datePublished\":\"2025-02-20T08:08:58+00:00\",\"dateModified\":\"2025-09-19T05:33:15+00:00\",\"mainEntityOfPage\":{\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/\"},\"wordCount\":678,\"commentCount\":0,\"publisher\":{\"@id\":\"https:\/\/www.kaysuns.com\/#organization\"},\"image\":{\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#primaryimage\"},\"thumbnailUrl\":\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp\",\"articleSection\":[\"Blogs\",\"Knowledge\"],\"inLanguage\":\"es\",\"potentialAction\":[{\"@type\":\"CommentAction\",\"name\":\"Comment\",\"target\":[\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#respond\"]}]},{\"@type\":\"WebPage\",\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/\",\"url\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/\",\"name\":\"N04400 Welding Precautions And Process Instructions\",\"isPartOf\":{\"@id\":\"https:\/\/www.kaysuns.com\/#website\"},\"primaryImageOfPage\":{\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#primaryimage\"},\"image\":{\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#primaryimage\"},\"thumbnailUrl\":\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp\",\"datePublished\":\"2025-02-20T08:08:58+00:00\",\"dateModified\":\"2025-09-19T05:33:15+00:00\",\"description\":\"UNS N04400 is a nickel-based alloy material with good welding performance. We introduce you to its welding precautions.\",\"breadcrumb\":{\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#breadcrumb\"},\"inLanguage\":\"es\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/\"]}]},{\"@type\":\"ImageObject\",\"inLanguage\":\"es\",\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#primaryimage\",\"url\":\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp\",\"contentUrl\":\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp\",\"width\":1081,\"height\":423,\"caption\":\"N04400-P1\"},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"Home\",\"item\":\"https:\/\/www.kaysuns.com\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Blogs\",\"item\":\"https:\/\/www.kaysuns.com\/category\/blog\/\"},{\"@type\":\"ListItem\",\"position\":3,\"name\":\"UNS N04400 Alloy Welded Pipe Welding Precautions And Process Instructions\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\/\/www.kaysuns.com\/#website\",\"url\":\"https:\/\/www.kaysuns.com\/\",\"name\":\"Stainless Steel Pipe and Fittings | KAYSUNS\",\"description\":\"Stainless Steel Pipe &amp; Fittings Manufacturer and Supplier in China\",\"publisher\":{\"@id\":\"https:\/\/www.kaysuns.com\/#organization\"},\"alternateName\":\"KAYSUNS\",\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\/\/www.kaysuns.com\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"es\"},{\"@type\":\"Organization\",\"@id\":\"https:\/\/www.kaysuns.com\/#organization\",\"name\":\"Kaysuns Industry Ltd.\",\"url\":\"https:\/\/www.kaysuns.com\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"es\",\"@id\":\"https:\/\/www.kaysuns.com\/#\/schema\/logo\/image\/\",\"url\":\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2019\/12\/cropped-neve-industrial-logo-1.png\",\"contentUrl\":\"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2019\/12\/cropped-neve-industrial-logo-1.png\",\"width\":52,\"height\":59,\"caption\":\"Kaysuns Industry Ltd.\"},\"image\":{\"@id\":\"https:\/\/www.kaysuns.com\/#\/schema\/logo\/image\/\"}},{\"@type\":\"Person\",\"@id\":\"https:\/\/www.kaysuns.com\/#\/schema\/person\/9dd889bbe4a74acafea3a8d6480ae741\",\"name\":\"admin\",\"image\":{\"@type\":\"ImageObject\",\"inLanguage\":\"es\",\"@id\":\"https:\/\/www.kaysuns.com\/#\/schema\/person\/image\/\",\"url\":\"https:\/\/www.kaysuns.com\/wp-content\/litespeed\/avatar\/121daf51eb7c2ccb4353fd41f53e3cbe.jpg?ver=1776937894\",\"contentUrl\":\"https:\/\/www.kaysuns.com\/wp-content\/litespeed\/avatar\/121daf51eb7c2ccb4353fd41f53e3cbe.jpg?ver=1776937894\",\"caption\":\"admin\"},\"sameAs\":[\"https:\/\/x.com\/Admin\"]}]}<\/script>\n<!-- \/ Yoast SEO plugin. -->","yoast_head_json":{"title":"N04400 Precauciones de soldadura e instrucciones de proceso","description":"El UNS N04400 es un material de aleaci\u00f3n a base de n\u00edquel con buenas prestaciones de soldadura. Le presentamos sus precauciones de soldadura.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/www.kaysuns.com\/es\/uns-n04400-precauciones-e-instrucciones\/","og_locale":"es_ES","og_type":"article","og_title":"N04400 Welding Precautions And Process Instructions","og_description":"UNS N04400 is a nickel-based alloy material with good welding performance. We introduce you to its welding precautions.","og_url":"https:\/\/www.kaysuns.com\/es\/uns-n04400-precauciones-e-instrucciones\/","og_site_name":"Stainless Steel Pipe and Fittings | KAYSUNS","article_published_time":"2025-02-20T08:08:58+00:00","article_modified_time":"2025-09-19T05:33:15+00:00","og_image":[{"width":1081,"height":423,"url":"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp","type":"image\/webp"}],"author":"admin","twitter_card":"summary_large_image","twitter_creator":"@Admin","twitter_misc":{"Escrito por":"admin","Tiempo de lectura":"4 minutos"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"Article","@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#article","isPartOf":{"@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/"},"author":{"name":"admin","@id":"https:\/\/www.kaysuns.com\/#\/schema\/person\/9dd889bbe4a74acafea3a8d6480ae741"},"headline":"UNS N04400 Alloy Welded Pipe Welding Precautions And Process Instructions","datePublished":"2025-02-20T08:08:58+00:00","dateModified":"2025-09-19T05:33:15+00:00","mainEntityOfPage":{"@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/"},"wordCount":678,"commentCount":0,"publisher":{"@id":"https:\/\/www.kaysuns.com\/#organization"},"image":{"@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#primaryimage"},"thumbnailUrl":"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp","articleSection":["Blogs","Knowledge"],"inLanguage":"es","potentialAction":[{"@type":"CommentAction","name":"Comment","target":["https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#respond"]}]},{"@type":"WebPage","@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/","url":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/","name":"N04400 Precauciones de soldadura e instrucciones de proceso","isPartOf":{"@id":"https:\/\/www.kaysuns.com\/#website"},"primaryImageOfPage":{"@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#primaryimage"},"image":{"@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#primaryimage"},"thumbnailUrl":"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp","datePublished":"2025-02-20T08:08:58+00:00","dateModified":"2025-09-19T05:33:15+00:00","description":"El UNS N04400 es un material de aleaci\u00f3n a base de n\u00edquel con buenas prestaciones de soldadura. Le presentamos sus precauciones de soldadura.","breadcrumb":{"@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#breadcrumb"},"inLanguage":"es","potentialAction":[{"@type":"ReadAction","target":["https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/"]}]},{"@type":"ImageObject","inLanguage":"es","@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#primaryimage","url":"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp","contentUrl":"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2025\/02\/N04400-P1-e1740038690471.webp","width":1081,"height":423,"caption":"N04400-P1"},{"@type":"BreadcrumbList","@id":"https:\/\/www.kaysuns.com\/uns-n04400-precautions-and-instructions\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Home","item":"https:\/\/www.kaysuns.com\/"},{"@type":"ListItem","position":2,"name":"Blogs","item":"https:\/\/www.kaysuns.com\/category\/blog\/"},{"@type":"ListItem","position":3,"name":"UNS N04400 Alloy Welded Pipe Welding Precautions And Process Instructions"}]},{"@type":"WebSite","@id":"https:\/\/www.kaysuns.com\/#website","url":"https:\/\/www.kaysuns.com\/","name":"Tubos y accesorios de acero inoxidable | KAYSUNS","description":"Fabricante y proveedor de tubos y accesorios de acero inoxidable en China","publisher":{"@id":"https:\/\/www.kaysuns.com\/#organization"},"alternateName":"KAYSUNS","potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/www.kaysuns.com\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"es"},{"@type":"Organization","@id":"https:\/\/www.kaysuns.com\/#organization","name":"Kaysuns Industry Ltd.","url":"https:\/\/www.kaysuns.com\/","logo":{"@type":"ImageObject","inLanguage":"es","@id":"https:\/\/www.kaysuns.com\/#\/schema\/logo\/image\/","url":"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2019\/12\/cropped-neve-industrial-logo-1.png","contentUrl":"https:\/\/www.kaysuns.com\/wp-content\/uploads\/2019\/12\/cropped-neve-industrial-logo-1.png","width":52,"height":59,"caption":"Kaysuns Industry Ltd."},"image":{"@id":"https:\/\/www.kaysuns.com\/#\/schema\/logo\/image\/"}},{"@type":"Person","@id":"https:\/\/www.kaysuns.com\/#\/schema\/person\/9dd889bbe4a74acafea3a8d6480ae741","name":"admin","image":{"@type":"ImageObject","inLanguage":"es","@id":"https:\/\/www.kaysuns.com\/#\/schema\/person\/image\/","url":"https:\/\/www.kaysuns.com\/wp-content\/litespeed\/avatar\/121daf51eb7c2ccb4353fd41f53e3cbe.jpg?ver=1776937894","contentUrl":"https:\/\/www.kaysuns.com\/wp-content\/litespeed\/avatar\/121daf51eb7c2ccb4353fd41f53e3cbe.jpg?ver=1776937894","caption":"admin"},"sameAs":["https:\/\/x.com\/Admin"]}]}},"_links":{"self":[{"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/posts\/48846","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/comments?post=48846"}],"version-history":[{"count":49,"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/posts\/48846\/revisions"}],"predecessor-version":[{"id":53387,"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/posts\/48846\/revisions\/53387"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/media\/48894"}],"wp:attachment":[{"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/media?parent=48846"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/categories?post=48846"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.kaysuns.com\/es\/wp-json\/wp\/v2\/tags?post=48846"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}